Substrate: 420D, 600D box cloth
Product examples: sun umbrella, awning, handbags, bags and so on
Product features: high hiding power, good adhesion to the luggage, plain, not easy to stick back.
Test items | Adhesion | Resistant to migration | Scratch resistance | Abrasion resistance | Resistant to rubbing | Acid resistance | Alkali resistance | Resistant to washing |
Test Results | excellent | 4-5level | 3-4level | 3-4level | 3-4level | 4-5level | 4-5level | 3-4level |
Product Specifications:
Project | Hue | Color concentration | Fineness | Viscosity | Gloss | Mobility | Solid content |
Technical Parameters | Refer to the color card | ≥80% | 7u below | 200-380p | 30-85 | 15-20mm/s | 30% |
Instructions for use:
Stencil: 150-300 mesh polyester screen printing plate
Scraping: It is recommended to use 65-85 degree polyurethane plastic scraping
Reference amount: 200 mesh screen printing is about 30 ㎡ / ㎏
Dry: natural evaporation dry (dry 7-15 minutes, dry for more than 24 hours) or 60 ℃ -80 ℃ baking 20-30min.
Selection of solvents: 719 quick-drying water, 718 dry water or 783 slow dry water, cyclohexanone, due to different printing environment temperature appropriate choice.
Screen cleaning: the choice of organic solvent cleaning (such as: washing water)
Precautions:
1, the use of solvent dilution of ink, please pay attention to the solubility of the solvent, if the solubility is too weak is prone to reverse the phenomenon of ink, which is necessary to use a strong solvent solution.
2, printed on the bottom of the PVC peritoneum bag cloth, due to PVC solvent resistance is poor, easy to cause printed materials when the pattern of sticky flowers, so pay attention to the ink when the drying situation, while avoiding excessive overlap.
3, printed on the bottom of the PVC peritoneum bag cloth, because PVC contains a large number of plasticizers, likely to cause color migration. Special attention should be paid to the use of better resistance to the permeability of the ink color.
4, the series is mainly used for the printing of luggage cloth, the general nylon cloth and smoother Oxford cloth may appear poor adhesion phenomenon before you do a good job before the rigorous testing.
5, the printing of some special nylon fabric, due to poor adhesion may be added to the amount of 5% -8% 9004 catalyst to improve the adhesion of the ink, add the catalyst ink in 8 hours run out, otherwise the ink may knot fast scrapped.
Product packaging: 1 kg loaded, 5 kg loaded, 20 kg loaded
Storage conditions: 5 ℃ -35 ℃ conditions for two years, to avoid strong light exposure, anti-contact strong acid, alkali.
Tips:
1, users in the use of this product, please read the instructions, and must test the suitability of different batches of ink, the actual test India, to confirm the qualified before use in bulk;
2, the above conditions in the tolerance test data for the test conditions under the test results, not as a guarantee value.